    physical & mechanical properties

    Units
    Maximum continuous operating temperature in air °C 1250
    Nominal composition % Ni 80
    Cr 20
    Density at 20°C g/cm³ 8.3
    Resistivity at 20°C µΩcm 109
    Thermal conductivity at 20°C W/mK 14.6
    Specific heat capacity at 20°C kJ/kgK 0.42
    Melting point (approx.) °C 1400
    Tensile strength Rm, 0.5 mm wire – annealed N/mm² 610
    Elongation at break, 0.5 mm wire - annealed % > 25

    temperature dependant factors

    Reference temperature: 20°C
    Temp °C 200 400 500 600 800 1000 1200
    Temp °F 392 752 932 1112 1472 1832 2192
    Resistivity Factor 1.009 1.018 1.03 1.039 1.056 1.068 1.073
    Coefficient of thermal expansion (10^6/K) 11 12 12 13 14 15

    The figures given in these tables represent nominal or typical values.

    Information contained within this technical data sheet is based upon the general experience of Scott Precision Wire Ltd and is believed to be correct at the time of issue.

    No warranty is given or is to be implied from the details above.